How to repair protective coating after installation of metal structures

After welding, inspect the joint and surrounding area.

Sections of metal structures may arrive at the site with a good coating, and after assembly, receive damage to welded joints, mounting holes and slinging points. The entry “perform touch-up” does not show either the location of the defect or the result of the repair. For acceptance, it is more useful to have an address sheet, in which each treated area can be found and checked before covering with casing or equipment.

Distinguish between three montage situations

After welding, inspect the connection and the surrounding area. Check the condition of the protective coating, the presence of splashes and flux residues, and the ability to prepare the surface along the entire perimeter. Processing only the visible side of the node does not confirm that protection has been restored on the reverse side. If there is no access there, this is a separate issue of organizing work.

At the slinging site, the boundaries of the damaged layer and the condition of the steel underneath are determined. Scratches of the coating and deformation of the element require different solutions. The coating does not restore the load-bearing capacity: if there are signs of metal damage, the suitability of the structure is first decided upon, and then anti-corrosion repairs are prescribed.

Near the mounting hole, check the edge, burrs and access to the surface near the fastener. In the statement, it is better to designate such a zone separately from the straight section of the beam. The word “beam” without the element number and side will not allow the receiver to understand where exactly the restoration was performed.

Make a record suitable for re-checking

For example, instead of “scratches on the posts,” you can write: “Pillar K-12, outer edge, area under the mounting grip,” attach a photo and mark the boundaries of the damage on the diagram. This is a sample site addressing; actual designations are taken from the object documentation.

The original coating and the condition of the base are added to the record. Repairing preserved galvanized steel is different from repairing new steel or a surface with old paint. For a suitable site, a system is selected, including zinc plating of metal structures on site. The composition forms a zinc layer with a protective effect after the specified metal preparation.

Assign responsibility for each1st stage

In a repair task, it is useful to separate the identification of the defect, the purpose of the system, execution and acceptance. The installation crew notes the damage; the person responsible for the decision specifies processing; the performer records the completed operations; The receiver compares the result with the task. Specific roles and order are assigned to a given object, without leaving a general point without a person in charge.

Supply is provided with the names of the agreed materials - zinc plating compounds and a compatible solvent. For each repair area, a connection must be maintained with the system actually applied. Replacing a solvent or finish requires checking compatibility, and not just matching the color of the future coating.

Provide access for acceptance

The first check is carried out on a prepared base: cleaning, degreasing, dust removal and accessibility of difficult areas are assessed. Weld seams and hard-to-reach places are pre-treated with a brush before the main application. The conditions and thickness of the coating are determined according to the technology of the selected system and the facility documentationta.

After drying, check for gaps and defects, measure the dry thickness, and assign the results to the same repair area. The same gray color does not prove the required thickness at the edge and near the seam. The area should be closed with equipment after the required control, as long as access to it is maintained.

When choosing a recovery method, check the manufacturer's documentation Zinker and the requirements of the facility. The statement is closed according to the actual accepted area: with a mark of completion, inspection results and a photograph that allows you to recognize the location. Then the remark after installation turns into a verifiable repair task, and does not disappear behind a general phrase about touch-up.

UP